Abstract

Aim: The purpose of this study was to evaluate and compare shear bond strength and ARI score of orthodontic brackets bonded with three different orthodontic adhesive systems with and without primer.
Objective: To assess and compare the shear bond strength and adhesive remnant index score of three different orthodontic adhesive systems with and without primer.
Materials and Methods: The samples comprised 150 healthy premolars extracted for orthodontic purposes. All the teeth were mounted on an acrylic block and divided into 5 groups (30 samples in each group). Group A (Transbond XT Primer + Adhesive); Group B (Transbond XT Adhesive); Group C (Bracepaste Primer + Adhesive); Group D (Bracepaste Adhesive); Group E (Aqualine LC Adhesive). Stainless steel (3M Unitek) premolar brackets were used. Once the brackets are bonded. The bonding strength values were measured by a universal testing machine.
Results: Distribution of mean values in Intergroup overall, pairwise, comparison of shear bond strength and in Intergroup overall and pairwise comparison of adhesive remnant index scores of three different orthodontic adhesive systems with and without primer, showed a highly statistically significant difference (p<0> Conclusion: Group A has got the best and the highest shear bond strength of all the groups. No statistically significant difference was seen between Group A and B; Group C and D have got the least shear bond strength. Group E has got clinically acceptable shear bond strength that is almost equal to that of Group A and B. Group A has got the best and the highest ARI score of 2 and 3 of all the groups. Group C and D have got the highest ARI score of 0 and 1.


Keywords : Shear bond strength, Adhesive remnant index score, Transbond XT primer, Transbond XT adhesive, Bracepaste adhesive, Aqualine LC adhesive.


How to cite : Shaikh S, Mirdehghan N, Kalia A, Hegde A, Joshi J, Khan A A, Comparison of shear bond strength and adhesive remnant index score of three different orthodontic adhesive systems with and without primer: An in vitro study. Int J Oral Health Dent 2024;10(3):166-173


This is an Open Access (OA) journal, and articles are distributed under the terms of the Creative Commons Attribution-NonCommercial-ShareAlike 4.0 License, which allows others to remix, tweak, and build upon the work non-commercially, as long as appropriate credit is given and the new creations are licensed under the identical terms.







Article History

Received : 18-05-2024

Accepted : 28-06-2024


View Article

PDF File   Full Text Article


Copyright permission

Get article permission for commercial use

Downlaod

PDF File   XML File   ePub File


Digital Object Identifier (DOI)

Article DOI

https://doi.org/10.18231/j.ijohd.2024.032


Article Metrics






Article Access statistics

Viewed: 104

PDF Downloaded: 23



Medical Abbreviation List